Shear Bond Strength of a Self-etching Primer after 10,000 and 20,000 Thermal Cycles
JOURNAL OF ADHESIVE DENTISTRY, vol.12, no.2, pp.117-122, 2010 (SCI-Expanded, Scopus)
- Publication Type: Article / Article
- Volume: 12 Issue: 2
- Publication Date: 2010
- Doi Number: 10.3290/j.jad.a17540
- Journal Name: JOURNAL OF ADHESIVE DENTISTRY
- Journal Indexes: Science Citation Index Expanded (SCI-EXPANDED), Scopus
- Page Numbers: pp.117-122
- Keywords: self-etching primer, thermocycling, bond strength, ORTHODONTIC BRACKETS, ADHESIVE SYSTEMS, GLASS-IONOMER, ENAMEL, CEMENT, TIME
- Ondokuz Mayıs University Affiliated: Yes
Abstract
Purpose: To determine the effects of thermocycling on shear bond strengths (SBSs) of a self-etching primer (SEP) after 10,000 and 20,000 thermal cycles. The tested hypothesis was that 10,000 and 20,000 thermal cycles would affect the bond strength of metal brackets bonded to enamel with the self-etching primer.